JIANGSU MITTEL STEEL INDUSTRIAL LIMITED

Jiangsu Mittel Steel Industrial Limited Supply all kinds of Stainless Steel Sheet/Plate/Coil/Round ,Flat ,Angle Bar/Stainless steel Seamless pipe /welded pipe /Elbow/Flange /Galvanized Steel sheet

Manufacturer from China
Verified Supplier
11 Years
Home / Products / Ship Steel Plate /

CCS DH36 Ship Steel Plate LR DH36 Shipbuilding Steel Plate ASTM A131 Gr Dh36

Contact Now
JIANGSU MITTEL STEEL INDUSTRIAL LIMITED
Visit Website
City:wuxi
Province/State:jiangsu
Country/Region:china
Contact Person:MrGao Ben
Contact Now

CCS DH36 Ship Steel Plate LR DH36 Shipbuilding Steel Plate ASTM A131 Gr Dh36

Ask Latest Price
Brand Name :Bao Steel Mittel
Model Number :DH36
Certification :SGS ISO MTC
Place of Origin :China
MOQ :500KGS
Price :750 USD/Ton
Payment Terms :L/C, T/T
Supply Ability :50000KGS
Delivery Time :14 Days After Received Deposit
Packaging Details :14 Days
Material :DH36
Width :500-3000mm
Length :2000-12000mm
Thickness :3-150mm
Condition :Hot Rolled
Classification :CCS LR GL ABS
more
Contact Now

Add to Cart

Find Similar Videos
View Product Description

DH36 shipbuilding steel plate is used for shipbuiling&platform.The shipbuilding steel plate grade DH36 is the high tensile strength steel.DH36 shipbuilding steel is the Hull structural steel,with it's good toughness properties, higher strength,strong corrosion-resistance,the processing properties,and welding properties.ASTM A131 DH36 steel plate can be used in the manufacture of the ship's hull structure whose weight is more than 10000 tons.

ABS DH36 Shipbuilding Steel Specification:
Thickness: 4mm to 260mm,
Width: 1200mm to 4000mm
Length: 3000mm to 18000mm.

ABS DH36 Shipbuilding Steel Application:
ABS DH36 Shipbuilding steel plates are mainly used for making the offshore oil drilling platform, the hull of ship building and ship repairing, the platform pipe joints and other components.

DH36 steel plate Chemical Composition %


Grade
C max Si max Mn P max S max Als min Ti max Cu max Cr
max
Ni
max
Mo
max
Nb V
DH36 0.18 0.50 0.90-1.60 0.035 0.035 0.015 0.02 0.35 0.20 0.40 0.08 0.02-0.05 0.05-0.10

Note: Generally speaking CE will be 0.40%. If the delivery condition is TMPC, the CE will be : ≤ 0.38% (thickness ≤ 50mm),≤0.40%( when the thickness >50-100). Ceq% =(C+Mn)/6+(Cr+Mo+V)/5+(Ni+Cu)/15.

DH36 steel plate Mechanical Property


Grade
Rm
(MPa)
Re(MPa) min A% min Akv/J min
DH36 490-630 355 21 E.T °C Thickness (mm)
-20 50 >50-70 >70-100
L C L C L C
34 24 41 27 50 34

Note: In the list , Rm: .tensile strength,Re: Yield strength,A%: elongation, E.T: experimental temperature,L: lengthways, C: crosswise.

DH36 steel plate Condition Of Delivery


Grade
Fine grains elements category The thickness of steel
≤ 12 >12.5-20 >20-25 >25-35 >35-50 >50-100
DH36 Nb+V or V Plate/
sheet
A(50) N(50),CR(50),TM(50) N(50),CR(25),TM(50)
Profile steel N(50),CR(50),TM(50),AR*(25) -
Al or Al+Ti Plate/
sheet
A(50) AR*(25) -
N(50),CR(50),TM(50) N(50),CR(25),TM(50)
Profile steel A(50) N(50),CR(50),TM(50),AR*(25) -

Note: 1. delivery condition: A =Any ; N=Normalized ; CR=Control Rolled ; TM=TMPC, Temperature - deformation control rolling; AR*= Can be hot rolled with the agreement of Classification Society ; CR*=Can be control rolled with the agreement of Classification Society .
2. The Figure in the ( ) means the sampling volume to do the impact test, the unit is Ton.(-) means without impact test.

DH36 steel plate Contrast in the different standard


ASTM A131M
TOCT 5521 BS LR GB712
DH36 D36 DH36

D36

CCS DH36 Ship Steel Plate LR DH36 Shipbuilding Steel Plate ASTM A131 Gr Dh36CCS DH36 Ship Steel Plate LR DH36 Shipbuilding Steel Plate ASTM A131 Gr Dh36CCS DH36 Ship Steel Plate LR DH36 Shipbuilding Steel Plate ASTM A131 Gr Dh36CCS DH36 Ship Steel Plate LR DH36 Shipbuilding Steel Plate ASTM A131 Gr Dh36CCS DH36 Ship Steel Plate LR DH36 Shipbuilding Steel Plate ASTM A131 Gr Dh36