Add to Cart
ASTM JIS GB DIN Standard Grade 303 Stainless Steel Bar / Hexagonal Steel Bar 2.4460
Product Description:
Product Name | stainless steel hexagon bar |
Standard | JIS, AISI, ASTM, GB, DIN |
Size | Diameter : S6-S65mm or as request |
Length | Normal long 4M, Or as your request |
Surface | Bright ,hairline finsh |
Technics | cold drawn and polishing |
Application | construction field, ships building industry, petroleum & chemical industries, war and electricity industries, food processing and medical industry, boiler heat exchanger, machinery and hardware fields ,etc. |
Packing | Export standard or as customers' requirement |
Delivery time | Within 15 working days, according to customers' quantities |
Payment | L/C or T/T |
MQQ | 1 Ton |
Quality | High Quality.SGS inspection is accepted if needed |
Productivity | 500 Tons/Month |
Attention | We will supply you good quality and bottom price and first-class service in china and hope to be your golden supplier |
Stainless Steel 303 is a free machining non-magnetic austenitic alloy specially designed for improved machinability while maintaining good mechanical and corrosion resistant properties. AISI 303 is cannot be hardened by heat treatment, but tensile and hardness can be increased by cold working with subsequent reduction in ductility.The sulfur addition which is responsible for the improved machining and galling characteristics of Grade 303 lowers its corrosion resistance to below that of Grade 304. However, fairly resistant to general atmospheric corrosion, general foodstuffs, sterilizing solutions, dyestuffs, most organic chemicals, but has very limited resistance to acids.
Elements | Cr | Ni | C | Si | Mn | P | S | Mo | Fe |
---|---|---|---|---|---|---|---|---|---|
% | min: 17.0 ,max:19.0 | min: 8.0 ,max: 10.0 | 0.15 max | 1.00 max | 2.0 max | 0.20 max | 0.15 min | 0.75 | balance |
Tensile Strength ksi (min.) | Yield Strength 0.2% Offset ksi (min.) | Elongation - % in 50 mm (min.) | Hardness (Brinell) MAX | Hardness (Rockwell B) MAX |
---|---|---|---|---|
75 | 30 | 35 | 228 | - |
Denstiy lbm/in3 | Coefficient of Thermal Expansion (min/in)-°F | Electrical Resistivity mW-in | Thermal Conductivity BTU/hr-ft-°F | Melting Range | |||||||
---|---|---|---|---|---|---|---|---|---|---|---|
at 68 °F | at 68 – 212°F | at 68 – 932°F | at 68 – 1450°F | at 68°F | at 212°F | at 392°F | at 752°F | at 1112°F | at 1472°F | at 68 – 212°F | - |
0.29 | 9.2 | 10.4 | 10.9 | 28.3 | 30.7 | 33.8 | 39.4 | 43.7 | 47.6 | 113.2 | 2552°F |
SAE / AISI | 303 |
UNS | S30300 |
EN Material Number | 1.4305 |
EN Material Name | X8CrNiS18-9 |
DIN Material Name | X8CrNiS18-9 |
JIS | SUS 303 |
BS | 202S 21 En58M |