Add to Cart
AISI 630 / 17-4PH / 1.4542 H1150 Specification ASTM A564 Stainless Steel Round Bar
17-4 stainless is an age-hardening martensitic stainless combining high strength with the corrosion resistance of stainless steel. Hardening is achieved by a short-time, simple low-temperature treatment. Unlike conventional martensitic stainless steels, such as type 410, 17-4 is quite weldable. The strength, corrosion resistance and simplified fabrication can make 17-4 stainless a cost-effective replacement for high strength carbon steels as well as other stainless grades.
At the solution treating temperature, 1900°F, the metal is austenitic but undergoes transformation to a low-carbon martensitic structure during cooling to room temperature. This transformation is not complete until the temperature drops to 90°F. Subsequent heating to temperatures of 900-1150°F for one to four hours precipitation strengthens the alloy. This hardening treatment also tempers the martensitic structure, increasing ductility and toughness.
Standards | Designation |
---|---|
ASTM | A 276 |
Length | Diameter |
---|---|
2-6m | 1.0mm~250mm |
Type | Certification |
---|---|
17-4 Stainless Steel Round Bar | ISO 9001:2008 |
Below you will find a brief overview of a number of stainless steel bar specifications. If you do not see a specification listed, please contact us.
BS | JIS | IS | DIN | ASTM | |
---|---|---|---|---|---|
Semi Free Cutting Steel | 15AM/8M | SMn433H,SUM 41 | 13S25/ | — | 1137,1140 |
Free Cutting Steel | EN-1A EN-1A L | SUM-23 SUM-24 L | 11C10S25 —— | 9SMn30 | 1212/ |
Stainless Steel Bar Specifications | |||
---|---|---|---|
ASTM A276 | This specification encompasses cold-finished or hot-finished bars, including rounds, squares, and hexagons, and hot-rolled or extruded shapes, such as angles, tees, and channels in the more commonly used types of stainless steels. | ||
ASTM A479 | This specification includes cold and hot finished stainless steel bars, including rounds, squares, and hexagons, and hot-rolled or extruded shapes such as angles, tees, and channels. | ||
ASTM A484 | This specification includes wrought stainless steel bars, shapes, forgings, and billets or other semi-finished materials, except wire, for forging. The materials are available in four types of conditions. | ||
ASTM A582 | This specification includes cold or hot finished bars, which are suitable for machining processes. This specification includes rounds, squares, and hexagons, from common types of stainless free-machining steels. | ||
ASTM B473 | This specification includes nickel alloy bar & wire, which can be produced in a solution-annealed condition, stabilized-annealed condition, or annealed condition. |
Our Grades :
AISI:
201, 202, 301, 302, 303, 304, 304H, 304L, 316, 316H, 316L, 309, 309S, 310, 310S, 316Ti, 317, 317L, 347, 321, 321H, 410, 416, 420, 430, 430F, 431, 440C, 630, 17-4PH, F51
DIN:
WNR1.4301, WNR1.4305, WNR1.4306, WNR1.4307, WNR1.4401, WNR1.4404, WNR1.4571, WNR1.4541, WNR1.4828, WNR1.4841, WNR1.4845, WNR1.4449, WNR1.4438, WNR1.4310, WNR1.4550, WNR1.4541, WNR1.4878, WNR1.4006, WNR1.4005, WNR1.4021, WNR1.4028, WNR1.4016, WNR1.4104, WNR1.4105, WNR1.4057, WNR1.4542, WNR1.4462
Ni | Cr | Mo | Mn | Cu | Si | C | Cb+Ta | S | P | Fe | |
---|---|---|---|---|---|---|---|---|---|---|---|
MIN | 3.0 | 15.0 | – | – | 3.0 | – | – | 5 x C | – | – |
– |
MAX | 5.0 | 17.5 | 0.50 | 1.0 | 5.0 | 1.0 | 0.07 | 0.45 | 0.03 | 0.04 | Balance |
Temperature, °F | 70 | 212 | 392 | 572 |
Coefficient of Thermal Expansion, in/in°F x 10-6 | – | 7.2 | 7.5 | 7.8 |
Thermal Conductivity Btu • ft/ft2 • hr • °F | 8.6 | 9.2 | 9.8 | 10.4 |
Modulus of Elasticity, psi X 106 | 29.0 | 28.1 | 27.0 | 26.1 |
Tensile Strength : Unit – ksi (MPa) , Minimum
Yeild Strength : 0.2 % Offset , Unit – ksi (MPa) , Minimum
Elongation : in 2″, Unit : % , Minimum
Hardness : Rockwell , Maximum
H 900* | H 925 | H 1025 | H 1075 | H 1100 | H 1150 | H 1150-M | |
Ultimate Tensile Strength, ksi | 200 | 190 | 170 | 165 | 150 | 145 | 125 |
0.2% Yield Strength, ksi | 185 | 175 | 165 | 150 | 135 | 125 | 85 |
Elongation % in 2" or 4XD | 14 | 14 | 15 | 16 | 17 | 19 | 22 |
Reduction of Area, % | 50 | 54 | 56 | 58 | 58 | 60 | 68 |
Hardness, Brinell (Rockwell) | 420 (C 44) | 409 (C42) | 352 (C 38) | 341 (C 36) | 332 (C 35) | 311 (C 33) | 277 (C 27) |
Impact Charpy V-Notch, ft – lbs | 15 | 25 | 35 | 40 | 45 | 50 | 100 |